Effect of hydrogen on the integrity of aluminium?oxide interface at elevated temperatures
Name
Effect of hydrogen.pdf
Size
736.35 KB
Format
Adobe PDF
Checksum (MD5)
69609363729c4d7f0f5d7c2269707304
Author(s) • • • • •
Li, Meng
Xie, De-Gang
Ma, Evan
Zhang, Xi-Xiang
Shan, Zhi-Wei
Li, Ju
Date Issued
February 2017
Journal
Nature Communications
Publisher
Nature Publishing Group
Citation
Li, Meng; Xie, De-Gang; Ma, Evan; Li, Ju; Zhang, Xi-Xiang and Shan, Zhi-Wei. “Effect of Hydrogen on the Integrity of Aluminium–oxide Interface at Elevated Temperatures.” Nature Communications 8 (February 2017): 14564 © 2017 The Author(s)
Version
Final published version
Abstract
Hydrogen can facilitate the detachment of protective oxide layer off metals and alloys. The degradation is usually exacerbated at elevated temperatures in many industrial applications; however, its origin remains poorly understood. Here by heating hydrogenated aluminium inside an environmental transmission electron microscope, we show that hydrogen exposure of just a few minutes can greatly degrade the high temperature integrity of metal–oxide interface. Moreover, there exists a critical temperature of ∼150 °C, above which the growth of cavities at the metal–oxide interface reverses to shrinkage, followed by the formation of a few giant cavities. Vacancy supersaturation, activation of a long-range diffusion pathway along the detached interface and the dissociation of hydrogen-vacancy complexes are critical factors affecting this behaviour. These results enrich the understanding of hydrogen-induced interfacial failure at elevated temperatures.
MIT Department
Massachusetts Institute of Technology. Department of Nuclear Science and Engineering
Terms of Use
Creative Commons Attribution 4.0 International License
Persistent DSpace Link
DOI of Published Version
https://doi.org/10.1038/ncomms14564