High-Performance and Traditional Multicrystalline Silicon: Comparing Gettering Responses and Lifetime-Limiting Defects
Name
HPMC-SiandMC-Si-IEEEJPV2016un-formatted.pdf
Size
5.23 MB
Format
Adobe PDF
Checksum (MD5)
02e960b1ae618a1c64afb44fe604c106
Author(s) • • • • • • • • •
Ekstrom, Kai E.
Autruffe, Antoine
Lai, Barry
Stokkan, Gaute
del Canizo, Carlos
Castellanos, Sergio
Jensen, Mallory Ann
Morishige, Ashley Elizabeth
Hofstetter, Jasmin
Yen, Patricia
Date Issued
April 2016
Journal
IEEE Journal of Photovoltaics
Publisher
Institute of Electrical and Electronics Engineers (IEEE)
Citation
Castellanos, Sergio et al. “High-Performance and Traditional Multicrystalline Silicon: Comparing Gettering Responses and Lifetime-Limiting Defects.” IEEE Journal of Photovoltaics 6, 3 (May 2016): 632–640 © 2016 IEEE
Version
Author's final manuscript
Abstract
In recent years, high-performance multicrystalline silicon (HPMC-Si) has emerged as an attractive alternative to traditional ingot-based multicrystalline silicon (mc-Si), with a similar cost structure but improved cell performance. Herein, we evaluate the gettering response of traditional mc-Si and HPMC-Si. Microanalytical techniques demonstrate that HPMC-Si and mc-Si share similar lifetime-limiting defect types but have different relative concentrations and distributions. HPMC-Si shows a substantial lifetime improvement after P-gettering compared with mc-Si, chiefly because of lower area fraction of dislocation-rich clusters. In both materials, the dislocation clusters and grain boundaries were associated with relatively higher interstitial iron point-defect concentrations after diffusion, which is suggestive of dissolving metal-impurity precipitates. The relatively fewer dislocation clusters in HPMC-Si are shown to exhibit similar characteristics to those found in mc-Si. Given similar governing principles, a proxy to determine relative recombination activity of dislocation clusters developed for mc-Si is successfully transferred to HPMC-Si. The lifetime in the remainder of HPMC-Si material is found to be limited by grain-boundary recombination. To reduce the recombination activity of grain boundaries in HPMC-Si, coordinated impurity control during growth, gettering, and passivation must be developed. Keywords: Defects; dislocation recombination activity; dislocations; eccentricity variation; high-performance multicrystalline silicon (HPMC-Si); minority-carrier lifetime; photovoltaics; recombination; synchrotron
MIT Department
Massachusetts Institute of Technology. Department of Mechanical Engineering
Terms of Use
Creative Commons Attribution-Noncommercial-Share Alike
Persistent DSpace Link
DOI of Published Version
https://doi.org/10.1109/JPHOTOV.2016.2540246