Gradient-morph LiCoO2 single crystals with stabilized energy density above 3400 W h L−1
Name
d0ee00231c.pdf
Size
8.31 MB
Format
Adobe PDF
Checksum (MD5)
3193a41beccbc882a597f253474dff06
Author(s) • • • • • • • • •
Zhu, Zhi
Yu, Daiwei
Shi, Zhe
Gao, Rui
Xiao, Xianghui
Waluyo, Iradwikanari
Ge, Mingyuan
Dong, Yanhao
Xue, Weijiang
Xu, Guiyin
Date Issued
May 2020
Journal
Energy & Environmental Science
Publisher
Royal Society of Chemistry (RSC)
Citation
Zhu, Zhi et al. "Gradient-morph LiCoO2 single crystals with stabilized energy density above 3400 W h L−1." Energy & Environmental Science 13, 6 (May 2020): 1865-1878. © 2020 The Royal Society of Chemistry
Version
Final published version
Abstract
The cycling stability of LiCoO[subscript 2] under high voltages (>4.5 V) was plagued by hybrid anion- and cation-redox (HACR) induced oxygen escape and uncontrolled phase collapse. With DEMS and in situ XANES mapping at the NSLS-II, we demonstrate that oxygen escape triggers irreversible transformations into “bad” surface phases that rapidly propagate inward. Enabling HACR but stopping global oxygen migration is key to a stable high-energy cathode. Therefore, we developed ∼10 μm single crystals with LiCoO[subscript 2] in the bulk smoothly transitioning to Co-free LiMn[subscript 0.75]Ni[subscript0.25]O[subscript 2] at the surface. By means of initial electrochemical formation, a semi-coherent LiMn[subscript 1.5]Ni[subscript 0.5]O[subscript 4] spinel-like shell was established in operando with little oxygen loss to integrally wrap the LiCoO[subscript 2] bulk. Then we obtained gradient-morph LiCoO[[subscript 2] single crystals to prevent the percolating migration of oxygen out of the particle and achieved enhanced HACR reversibility at high voltages. The gradient-morph HACR cathode undergoes substantially stabilized cycling when charged to above 4.6 V, and hence a stable cyclic volumetric energy density of >3400 W h L−1 has been achieved in a pouch full-cell coupled with a commercial graphite anode and lean electrolyte (2 g A h−1), exhibiting up to 2906 W h L−1 even after 300 cycles.
MIT Department
Massachusetts Institute of Technology. Department of Nuclear Science and Engineering
Massachusetts Institute of Technology. Department of Materials Science and Engineering
Massachusetts Institute of Technology. Department of Electrical Engineering and Computer Science
Terms of Use
Creative Commons Attribution 3.0 unported license
Persistent DSpace Link
DOI of Published Version
https://doi.org/10.1039/D0EE00231C