Post-Depositional Alteration of Calcium Carbonate Phases in Archaeological Ceramics: Depletion and Redistribution Effects
Name
minerals-11-00749-v3.pdf
Size
9.8 MB
Format
Unknown
Checksum (MD5)
2021242c9d237c073d040f0a03b06f10
Author(s) • • • •
Gilstrap, William D.
Meanwell, Jennifer L.
Paris, Elizabeth H.
López Bravo, Roberto
Day, Peter M.
Date Issued
July 2021
Journal
Minerals
Publisher
MDPI AG
Citation
Minerals 11 (7): 749 (2021)
Version
Final published version
Abstract
The final stage in the life history of prehistoric pottery prior to archaeological recovery is usually the longest, and frequently the most dynamic. The remains of archaeological ceramics spend hundreds to thousands of years deposited within the upper layers of the earth’s crust where they encounter the same diagenetic environmental processes as the surrounding natural materials. Harsh conditions of subterranean environments induce physical stresses and chemical reactions, causing alterations of ceramic structure and composition. This is especially true of carbonate-rich ceramics, as carbonate phases are soluble when deposited within acidic environments. This paper examines common carbonate depletion and accretion effects of post-depositional environments on ancient ceramics from two rather different geological and archaeological contexts: Mesoamerica and the Mediterranean. Potters in both regions produce vessels with carbonate-rich materials—clays, calcite, limestone—that alter due to long exposure to low-pH sediments and continual water table fluctuations. Ceramic petrography is employed to identify traces of carbonate alterations within ceramic microstructure and to characterize fabrics. Elemental compositions of the same sherds are characterized through either scanning electron microscopy coupled with energy-dispersive spectrometry (SEM-EDS), inductively coupled plasma mass spectrometry and optical emission spectrometry (ICP-MS/OES) or neutron activation analysis (NAA). This method enabled comparison of the differing effects of post-depositional alteration of carbonate phases on bulk composition signatures commonly used to determine provenance.
MIT Department
Center for Materials Research in Archaeology and Ethnology
Terms of Use
Creative Commons Attribution
Persistent DSpace Link
DOI of Published Version
https://doi.org/10.3390/min11070749