Strain Shielding from Mechanically Activated Covalent Bond Formation during Nanoindentation of Graphene Delays the Onset of Failure

Author(s)
Kumar, Sandeep; Parks, David Moore
Thumbnail
DownloadParks_Strain Shielding.pdf (6.292Mb)
OPEN_ACCESS_POLICY

Open Access Policy

Creative Commons Attribution-Noncommercial-Share Alike

Terms of use
Creative Commons Attribution-Noncommercial-Share Alike http://creativecommons.org/licenses/by-nc-sa/4.0/
Metadata
Show full item record
Abstract
Mechanical failure of an ideal crystal is dictated either by an elastic instability or a soft-mode instability. Previous interpretations of nanoindentation experiments on suspended graphene sheets, however, indicate an anomaly: the inferred strain in the graphene sheet directly beneath the diamond indenter at the measured failure load is anomalously large compared to the fracture strains predicted by both soft-mode and acoustic analyses. Through multiscale modeling combining the results of continuum, atomistic, and quantum calculations, and analysis of experiments, we identify a strain-shielding effect initiated by mechanochemical interactions at the graphene–indenter interface as the operative mechanism responsible for this anomaly. Transmission electron micrographs and a molecular model of the diamond indenter’s tip suggest that the tip surface contains facets comprising crystallographic {111} and {100} planes. Ab initio and molecular dynamics (MD) simulations confirm that a covalent bond (weld) formation between graphene and the crystallographic {111} and {100} facets on the indenter’s surface can be induced by compressive contact stresses of the order achieved in nanoindentation tests. Finite element analysis (FEA) and MD simulations of nanoindentation reveal that the shear stiction provided by the induced covalent bonding restricts relative slip of the graphene sheet at its contact with the indenter, thus initiating a local strain-shielding effect. As a result, subsequent to stress-induced bonding at the graphene–indenter interface, the spatial variation of continuing incremental strain is substantially redistributed, locally shielding the region directly beneath the indenter by limiting the buildup of strain while imparting deformation to the surrounding regions. The extent of strain shielding is governed by the strength of the shear stiction, which depends upon the level of hydrogen saturation at the indenter’s surface. We show that at intermediate levels of hydrogen saturation the strain-shielding effect can enable the graphene to support experimentally determined fracture loads and displacements without prematurely reaching locally limiting states of stress and deformation.
Date issued
2015-01
URI
http://hdl.handle.net/1721.1/97691
Department
Massachusetts Institute of Technology. Department of Mechanical Engineering
Journal
Nano Letters
Publisher
American Chemical Society (ACS)
Citation
Kumar, Sandeep, and David M. Parks. “Strain Shielding from Mechanically Activated Covalent Bond Formation During Nanoindentation of Graphene Delays the Onset of Failure.” Nano Lett. 15, no. 3 (March 11, 2015): 1503–1510.
Version: Original manuscript
ISSN
1530-6984
1530-6992

Collections
  • MIT Open Access Articles

Browse

All of DSpaceCommunities & CollectionsBy Issue DateAuthorsTitlesSubjectsThis CollectionBy Issue DateAuthorsTitlesSubjects

My Account

Login

Statistics

OA StatisticsStatistics by CountryStatistics by Department
MIT Libraries
PrivacyPermissionsAccessibilityContact us
MIT
Content created by the MIT Libraries, CC BY-NC unless otherwise noted. Notify us about copyright concerns.